The paint system decides how long a metal roof keeps its color. Here's how the common finishes compare.

choosing siding colors

The layers of a painted panel

A painted metal panel is more than paint. From the inside out:

  1. Steel core: the strength
  2. Metallic coating: zinc or aluminum-zinc, the main rust protection
  3. Pretreatment and primer: help the paint bond
  4. Top coat: the color, and the first line of defense against sun and weather
  5. Backer coat: a thin coat on the underside

Common finishes

Finish What it is Fade and chalk resistance Relative cost Typical paint warranty
Galvanized (bare) Zinc-coated steel, no paint n/a $ Coating warranty only
Bare aluminum-zinc coated Aluminum-zinc coated steel, no paint n/a $ Coating warranty only
Polyester Basic paint system Fair $ Shorter or limited
SMP (silicone-modified polyester) The most common painted finish Good $$ Commonly 20 to 40 years
PVDF (fluoropolymer) Premium paint with the highest fluoropolymer content Best $$$ Commonly 30 to 40+ years

Warranty terms vary by manufacturer and location. Warranty details for your products are in your account.

SMP or PVDF?

SMP is a hard, durable paint at a moderate price. It's the standard for most homes, barns, shops and metal buildings. It may fade and chalk more than PVDF over decades, especially in bright reds, blues and dark colors.

PVDF holds its color and gloss the longest. It's common on architectural standing seam, commercial buildings, coastal projects and anywhere color consistency matters for decades. It's softer than SMP, so it needs a little more care during installation.

Fading and chalking

  • Fading is a slow loss of color from sunlight.
  • Chalking is a fine powder that forms on the surface as paint weathers.

Paint warranties usually limit how much fading and chalking can happen over a set number of years. Light colors and earth tones show less change than deep, bright colors.

Coastal and corrosive areas

Salt air, fertilizer, animal waste and industrial fumes speed up corrosion. In these areas, look at:

  • Heavier metallic coatings
  • PVDF paint
  • Aluminum panels near the coast
  • Stainless or coated fasteners

Some warranties exclude or limit coverage near saltwater. Check the distance limits before ordering.